We use aluminum every day. It is used in cars, homes, factories, and other places. There are many reasons behind aluminum’s popularity. One of the most crucial reasons is the aluminum’s strength against weight ratio. Another critical factor here is the “Bod tání hliníku.” becauase lot of aluminum parts that may need casting, in that case we need to know what is melting point of aluminum alloy so that we could set up the right temperature for our melting oven.
Aluminum typically has a low melting point compared to SS or CS. Because of this, it is easy to process and handle and is widely used in many industries. Houses, cars, aircraft, computers, and many others are typical examples. of course lightweight is another advantages of alumnum alloy, that is reason many of car parts are using tlakové lití hliníku products.
Aluminum is also very resistant to corrosion. But if you’re working with aluminum, there’s a critical point to consider: The Melt Point of Aluminum. Streigth of aluminum and surface finish of aluminum. All of those are very important when you plan to sue aluminum or alumnum alloy for your project. in today we are focus on aluminum melting point topic, of course you could go to advantages and disadvantages of aluinum die casting to know more about aluminum alloy material.
In general, aluminum’s melting teplota is 660.32 degrees Celsius. Most processing and handling jobs are conducted based on this value. Some conventional processes include welding, casting, extrusion, and heat treatment. This information is essential to engineers and manufacturers to set the correct temperatures. Here, the melting point of aluminum can be used as a threshold.
The aluminum melting point is involved in all stages of aluminum processing, from heating to other activities. It impacts issues with storage, transport, and even the material to be used. With aluminum alloys, this threshold varies slightly. Therefore, when looking for aluminum as a material to use for a particular project, you may want to to know what temp does aluminum melt.
Other other handle, different type of aluminum have little different melting teplota as well, for example aluminum 6061 will have differnt melting point than aluminum 7075, when use aluminum material for your project you need to think about which type of aluminum do you plan to use, if you are not sure about this, you are welcome to contact us, we are a China aluminum die casting manufacturer that have been working in aluminum alloy prouucts over 18 years, we can suggest you the right aluminum material according to your requirement.
Tento článek je o tématu "Co je Bod tání hliníku." Bude se zabývat především širokým rozsahem bodů tání hliníku. Také se dozvíte, jaké faktory tuto hodnotu ovlivňují. Věříme, že vám tento článek pomůže získat více informací o různých druzích hliníku a jejich bodech tání.

Jaký je bod tání hliníku?
Na stránkách bod tání hliníku se začíná zkapalňovat. V tomto okamžiku dochází k významné přeměně materiálu. Tuto přeměnu můžete pozorovat, pokud proces pozorujete v nádobě. V bodě tání začíná hliník přecházet z pevné nebo tuhé formy do kapalného stavu.
U hliníku k této změně dochází přesně při teplotě 660,3 °C neboli 1220,54 °C. Proces tavení má obvykle tři hlavní fáze. Nejprve zůstává hliník v pevném stavu, který se pohybuje pod teplotou 660,32 °C. Za druhé hliník přechází do bodu přechodu, který je při teplotě 660,32 stupňů Celsia. Nakonec se hliník mění v kapalinu, když je teplota vyšší než 660,32 stupně Celsia.
Může to být jen číslo, ale v mnoha aplikacích má zásadní význam. Konstruktérům poskytuje spolehlivé vodítko pro manipulaci, zpracování a použití hliníku. Tento bod tání se však může lišit v závislosti na typu hliníku.
Obecně můžeme hliník rozdělit do tří základních kategorií: komerční, binární a slitiny pro odlévání.

Řada komerčních slitin
Komerční slitiny jsou základními třídami hliníku v této rodině. Jedná se o "volbu" pro každodenní použití. Lidé je hojně využívají ve stavebnictví, dopravě nebo při balení. Tyto slitiny kombinují hliník s různými prvky, jako je hořčík nebo křemík. Hlavním důvodem tohoto míchání je zajištění pevnosti a odolnosti proti korozi. Jsou spolehlivé, univerzální a používají se všude.
Název slitiny | Bod tání hliníku |
Slitina 2024 | 500 až 635 °C |
Slitina Al 3003 | 643 až 654 °C |
Hliníková slitina 6061 | 582 až 652 °C |
Slitina Al 7075 | 477 až 635 °C |
Hliníková slitina A356 | 667 až 796 °C |
Systémy binárních slitin
Systémy binárních slitin jsou jednoduché, ale účinné. Kombinují hliník pouze s jedním prvkem, proto název "binární". Tyto slitiny se zaměřují na posílení specifických vlastností tím, že udržují směs jednoduchou. Pokud potřebujete něco lehkého, ale velmi robustního, jako jsou binární slitiny, odvedou zde nejlepší práci. Tyto hliníkové slitiny se hojně používají ve speciálních strojích a elektronice.
Název slitiny | Bod tání hliníku |
Al-Cu | 548°C |
Al-Si | 577°C |
Al-Mg | 600°C |
Al-Zn | 382°C |
Die Casting Aluminum Alloys
Aluminum Casting alloys are used to feed molten aluminum into formy pro tlakové lití. They have a very high melting range. These alloys are typically easy to shape and work well under high temperatures. People use them for intricate designs or precision casting alloy parts. These aluminum alloys are built to withstand heat and pressure. People widely use them in high-stress environments.
Below are some of aluminum alloys with their melting points:
Název slitiny | Bod tání hliníku |
Hliníková slitina A360 | 1030 až 1100 °C |
A380 Hliníková slitina | 1000 až 1100 °C |
Slitina hliníku A413 | 1070 až 1080 °C |
Why Is Aluminum Melting Temperature Important?
Na stránkách bod tání hliníku affects almost every aspect of its use in manufacturing. It tells you exactly when the aluminum alloy will soften and mold. Understanding the melting point keeps your process efficient and safe when handling aluminum. You must understand the melting temperature of aluminum for three main reasons.
Manipulace s materiálem
In material handling, knowing the melting point of aluminum can prevent costly errors. When aluminum is near its melting temperature, it needs extra care. Overheating is a common problem when handling aluminum. Sometimes, you might find defects like warping or degradation, which are common symptoms of overheating. In this case, if you are aware of the bod tání hliníku, you can reduce this at the highest level.
Ochrana povrchu
Ochrana povrchu závisí také na znalosti teploty. Když se hliník blíží k bodu tání, stává se náchylnějším k poškození povrchu. Povlaky a eloxované vrstvy chrání povrch hliníku, ale mohou se poškodit, pokud překročí určité teploty. Musíte tedy znát specifickou teplotu tání hliníku.
Vybavení a nástroje
Každý nástroj používaný na hliník je ovlivněn jeho bodem tání. Vysoké teploty obvykle vyžadují speciální nástroje, které se při práci v blízkosti hranice tání hliníku nezničí. Používání správného vybavení pro horký hliník umožňuje bezpečnější práci a minimalizuje opotřebení nástrojů.
Body tání běžných slitin hliníku
Hliníkové slitiny jsou v dnešním světě nejpoužívanějším hliníkem. Mají všechno, od lehké pevnosti až po odolnost proti korozi. Jedním z klíčových faktorů, který zde vyniká, je však bod tání. Již víte, proč je znalost bodu tání hliníku klíčová. Všimněte si, že každá slitina má svůj jedinečný rozsah tání.
Slitina | 2024 | 3003 | 5052 | 6061 | 7075 |
Hustota | 2,78 g/cc | 2,73 g/cc | 2,68 g/cc | 2,7 g/cc | 2,81 g/cc |
Bod tání | 502 - 638°C | 643 - 654°C | 607 - 649°C | 582 - 652°C | 477 - 635°C |
Bod tání hliníku 2024
Aluminum 2024 is known for its unique strength and fatigue resistance. Due to its strength-to-weight ratio, this alloy is frequently used in aerospace applications. The melting temperature for aluminum 2024 is between 500 degrees and 638 degrees Celsius.
Aluminum 2024 isn’t the best for corrosion resistance, so it’s often paired with a protective layer or treated with anodizing. If you’re considering heat-treating this alloy, note that its melting temp needs precision. A slight misstep might compromise its structural integrity.
Komponenta | Hmotnost % |
Al (hliník) | 90.7 – 94.7 |
Cr (chrom) | 0.1 |
Cu (měď) | 4.9 |
Fe (železo) | 0.5 |
Mg (hořčík) | 1.2 – 1.8 |
Mn (mangan) | 0.3 – 0.9 |
Ostatní (každý) | 0.05 |
Ostatní (celkem) | 0.15 |
Si (křemík) | 0.5 |
Ti (titan) | 0.15 |
Zn (zinek) | 0.25 |
Bod tání hliníku 3003
Pokud potřebujete větší odolnost proti korozi a slušnou pevnost, zvažte tuto hliníkovou slitinu. Její bod tání se pohybuje mezi 643 a 654 stupni Celsia, což z ní činí převažující volbu pro aplikace při relativně vysokých teplotách.
Unlike 2024, aluminum 3003 is not very strong. However, it is malleable and easy to work with. Its higher melting temperature makes it ideal for handling welding and bending work.
Komponenta | Hmotnost % |
Mn (mangan) | 1.1 – 1.5 |
Fe (železo) | 0.7 |
Cu (měď) | 0.2 |
Mg (hořčík) | 0.05 |
Si (křemík) | 0.6 |
Zn (zinek) | 0.1 |
Al (hliník) | Bilance |
Ostatní (každý) | 0.15 |
Bod tání hliníku 5052
If you are looking for an aluminum alloy with both strength and flexibility, Aluminum 5052 is the best choice. This alloy material is prevalent for superior corrosion resistance. People mostly prefer this aluminum alloy for marine environments and fuel tanks. This aluminum melting point generally ranges from 607 to 649 degrees Celsius.
Hliník 5052 nereaguje dobře na tepelné zpracování za účelem zvýšení pevnosti. Je však velmi dobře zpracovatelný. Lze jej snadno tvarovat, ohýbat nebo svařovat, takže je velmi univerzální pro různé aplikace.
Komponenta | Hmotnost % |
Al (hliník) | 95.7 – 97.7 |
Cr (chrom) | 0.15 – 0.35 |
Cu (měď) | 0.1 |
Fe (železo) | 0.4 |
Mg (hořčík) | 2.2 – 2.8 |
Mn (mangan) | 0.1 |
Ostatní (každý) | 0.05 |
Ostatní (celkem) | 0.15 |
Si (křemík) | 0.25 |
Zn (zinek) | 0.1 |
Bod tání hliníku 6061
Hliník 6061 je ideální pro konstrukční aplikace. Je pevný, odolný proti korozi a lze jej svařovat. Teplota tání slitiny hliníku 6061 se obvykle pohybuje mezi 582 a 652 stupni Celsia. Tento materiál také nabízí určitou flexibilitu. Je to nejen odolná, ale také velmi lehká hliníková slitina.
Hliník 6061 se hojně používá na výrobu rámů kol, mostů a strojních součástí. Dokáže vyvážit pevnost, tvarovatelnost a svařitelnost.
Al (hliník) | 95.8 – 98.6 |
Cr (chrom) | 0.04 – 0.35 |
Cu (měď) | 0.15 – 0.4 |
Fe (železo) | 0.7 |
Mg (hořčík) | 0.8 – 1.2 |
Mn (mangan) | 0.15 |
Ostatní (každý) | 0.05 |
Ostatní (celkem) | 0.15 |
Si (křemík) | 0.4 – 0.8 |
Ti (titan) | 0.15 |
Zn (zinek) | 0.25 |
Bod tání hliníku 7075
If you are looking for more strength, aluminum 7075 is an option you can consider. This aluminum alloy is famous for its high strength-to-weight ratio. It is often used in aircraft and automotive applications. This aluminum melting point lies between 477 and 635 degrees Celsius.
Nižší rozsah tání má však i své nevýhody. Hliník 7075 je sice velmi pevný, ale není tak odolný proti korozi jako jiné slitiny, například 5052. Chcete-li maximalizovat jeho výkon, můžete jej opatřit nátěrem nebo eloxovat, abyste ochránili povrch před oxidací. Jeho nižší teplota tání také znamená, že je třeba s ním při tepelném zpracování zacházet opatrně.
Komponenta | Hmotnost % |
Al (hliník) | 87.1 – 91.4 |
Cr (chrom) | 0.18 – 0.28 |
Cu (měď) | 1.2 – 2 |
Fe (železo) | 0.5 |
Mg (hořčík) | 2.1 – 2.9 |
Mn (mangan) | 0.3 |
Ostatní (každý) | 0.05 |
Ostatní (celkem) | 0.15 |
Si (křemík) | 0.4 |
Ti (titan) | 0.2 |
Zn (zinek) | 5.1 |
Faktory ovlivňující bod tání hliníku
Na stránkách bod tání hliníku není pevně stanovena. Ovlivňuje ji několik faktorů, včetně jejího složení, fyzikálních vlastností a výrobních postupů. Tyto faktory do značné míry určují, kdy hliník přejde z pevného stavu do kapalného.
Složení slitiny nebo úrovně čistoty
Teplota tání čistého hliníku se obvykle pohybuje kolem 660,32 °C. V průmyslu však není čistý hliník vždy praktický. Často se leguje s jinými prvky, aby se zvýšila jeho pevnost, pružnost a odolnost.
Do hliníku se často přidávají prvky jako měď, hořčík, křemík a zinek. Tyto prvky pomáhají hliníku odolávat různým aplikacím, ale mění jeho chování při tavení. Například teplota tání slitiny hliníku 6061 je 582 až 652 stupňů, což je méně než u čistého hliníku. Ve slitině hliníku 6061 najdete chrom, měď, železo, hořčík a další.
Na rozdíl od čistých kovů nemají slitiny obvykle jediný ostrý bod tání. Místo toho mají určitý rozsah teplot tání. Materiál se taví při nižší teplotě a před úplným zkapalněním přechází do kašovité fáze. Tento rozsah se liší podle složení a může ovlivnit proces, ve kterém se slitina používá.
Metody tepelného zpracování
Tepelné zpracování může změnit tvar hliníku na molekulární úrovni. Někdy se může stát, že se váš výrobek po odlití nebo vytlačení nebude chovat stejně jako předtím. V takovém případě působí tepelné zpracování na vlastnosti hliníku jako resetovací tlačítko. Teplotu tání hliníku ovlivňuje několik typů metod tepelného zpracování.
Hašení
Kalení zahrnuje zahřátí hliníku na určitou teplotu a jeho následné ochlazení. Ačkoli kalení nemusí nutně snížit teplotu tání hliníku, mění jeho mikrostrukturu. V některých případech se může kalený hliník tavit méně rovnoměrně.
Žíhání
Žíhání je opakem kalení. Zahřívá hliník a poté jej pomalu ochlazuje. V důsledku toho jsou hliníkové díly měkčí a tvárnější. Žíhání snižuje vnitřní pnutí. Může vytvořit konzistentnější chování při tavení. Protože žíhaný hliník nabízí vysokou přesnost, často se používá při odlévání kovů.
Zpevnění srážkami
Tento proces zvyšuje pevnost hliníkových slitin jejich zahříváním a ochlazováním. Tato metoda tepelného zpracování se provádí ve velmi kontrolovaném prostředí.
Srážkové vytvrzování obecně nesnižuje teplotu tání. Zvyšuje však teplotní stabilitu.
Fyzické vlastnosti
Fyzikální vlastnosti také výrazně ovlivňují bod tání hliníku. Mezi rozhodující faktory patří velikost zrn, úroveň napětí a velikost vzorku.
Velikost zrna
Velikost zrn v kovech označuje velikost jednotlivých krystalů, které se v kovu tvoří. Drobná a velká zrna se při tavení chovají odlišně.
Menší mohou mírně zvýšit bod tání, protože přidávají pevnost. Větší zrna však mohou teplotu tání snížit. Všimněte si, že s hliníkem s většími zrny se snadno pracuje při nižších teplotách.
Napětí a deformace
Hliník můžete podle potřeby namáhat, ohýbat, natahovat nebo stlačovat. Při těchto činnostech dochází ke změně vnitřní struktury hliníkového dílu.
Vnitřní energie z pnutí v namáhaném hliníku může snížit energii potřebnou k zahájení tavení, takže se může tavit při nižších teplotách.
Velikost vzorku
Záleží také na velikosti vzorku, zejména při laboratorním testování bodů tání. Velké vzorky mají obvykle konzistentnější chování při tání. Na druhou stranu menší vzorky mohou vykazovat proměnlivé rozsahy tání v důsledku vlivu plochy povrchu.
Chemické vlastnosti
Jak víte, rozdíl mezi čistým hliníkem a jeho slitinami. Každý z těchto hliníků může poskytovat jedinečné chemické vlastnosti. V důsledku toho můžete získat různé tavení každého hliníku.
Oxidace však ovlivňuje také teplotu tání hliníku. Ačkoli je hliník přirozeně odolný proti korozi, může v náročných podmínkách stále korodovat. Korozní vrstva může ovlivnit chování hliníku při tavení.
Bod tání v průmyslovém použití a zpracování
Bod tání hliníku je nezbytný téměř v každé továrně na hliník. Tam, kde dochází ke zpracování nebo výrobě hliníkových dílů, je bod tání hliníku rozhodujícím faktorem. V této části se seznámíte s některými průmyslovými aplikacemi.
Tepelné zpracování
Heat treatment is one of the most common applications where the melting point is critical. This method typically changes aluminum strength, flexibility, or durability. You can’t use a higher temperature above the melting point or do it at very low temperatures when heat-treating aluminum. You must maintain an optimal temperature for heat treatment.
Znalost teploty tání hliníku obvykle umožňuje nastavit přesné parametry. To je nezbytné zejména pro žíhání a srážecí kalení.
Odlévání kovů
Odlévání kovů také do značné míry závisí na teplotě tání hliníku. Mezi běžné metody odlévání patří lití pod tlakem, lití do trvalých forem a lití do písku.
Odlévání hliníku zahrnuje zahřátí kovu do roztaveného stavu a jeho nalití do forem pro vytvoření přesného tvaru konečného dílu. Pokud se použije příliš mnoho tepla, dojde k narušení celistvosti formy. Na druhou stranu přílišné ochlazení může mít za následek neúplné výplně nebo viditelné vady.
Ať už použijete jakoukoli metodu, cílem je zajistit hladké nalévání.
Tlakové lití
Die casting is one of the most popular methods for shaping aluminum. This process forces molten aluminum into a die casting mold cavity at high pressure.
Temperature control is vital in tlakové lití hliníku manufacturing process. Casting parts might weaken if the temperature drifts too close to aluminum’s melting point. In contrast, you risk damaging the die if the temperature is too high. You want uniformity in every casting. In this case, temperature stability can help you get there.
To working with aluminum die casting process, you need to know the melting point of aluminum for the most of aluminum alloys, those including ADC12, A356, A380, LM25, etc.
Odlévání do trvalých forem
Odlévání do trvalých forem se liší od lití pod tlakem. Jak už název napovídá, tato metoda používá trvalou formu, kterou lze použít vícekrát. Při výběru materiálu formy hraje významnou roli teplota tání hliníku. Protože forma přichází do styku s roztaveným hliníkem, musí odolávat teplu.
Pro zpracování hliníku nepotřebujete materiál formy s vysokou tepelnou odolností. Můžete pečlivě zvolit levnější materiál formy, který odolá teplu s vaším pracovním materiálem. Na druhou stranu, pokud je materiál nekvalitní, rychleji se opotřebuje. V každém případě můžete počítat s vyššími náklady a zažijete více prostojů.
Odlévání do písku
Odlévání do písku je nejjednodušší a nejběžnější metoda. Když se hliník nalije do pískové formy, jeho bod tání určuje, jak rychle nebo pomalu se ochladí. Pokud hliník chladne příliš rychle, nemusí formu vyplnit. Příliš pomalé chlazení může ovlivnit strukturální integritu dílu a vést k mnoha problémům.
Proces vytlačování
Vytlačováním se horký hliníkový polotovar protlačí přes matrici a vytvoří se specifické tvary. Stroj hliník průběžně zahřívá. V tomto případě je nezbytné si uvědomit, že proces vytlačování nemůže překročit bod tání hliníku. To je nezbytné, protože chování hliníku se po dosažení bodu tání stává nepředvídatelným. Z tohoto důvodu mohou vaše hliníkové díly získat nekonzistentní tvary nebo dokonce selhat.
Svařování hliníku
Svařování hliníku je složité, aniž byste se museli starat o body tání. Hliník má vysokou tepelnou vodivost, což znamená, že se rychle zahřívá a stejně rychle chladne. Aby svařování fungovalo, musí hliník dosáhnout správné teploty, aby se spojil, aniž by se zcela roztavil.
Často kladené otázky
Který kov se rychle taví?
Rychlost tání obvykle závisí na jeho tepelné vodivosti. Měď a hliník mají obecně velmi vysokou tepelnou vodivost. Zatímco hliník má teplotu tání 660,32 stupně, měď má hodnotu 1085 stupňů Celsia.
Jaký je bod tání čistého hliníku?
Teplota tání čistého hliníku je 660,32 °C, což je kritické číslo pro každého, kdo pracuje s hliníkem. Čistý hliník je však méně oblíbený než hliníkové slitiny.
Is It Possible to Determine the Identity of The Impurities Based on Melting Temperature?
Yes, you can often get clues about impurities by observing melting behavior. Indeed, it’s the quickest and easiest solution to find the impurities. Pure metal, like aluminum, has a sharp melting temperature. However, if there are impurities, the melting point can drop, or the metal may not reach a border temperature range.
Která hliníková slitina má nejnižší bod tání?
Slitina hliníku 7075 má nejnižší bod tání, a to mezi 477 a 635 stupni Celsia. Díky tomuto nižšímu rozsahu tání je tato slitina velmi vhodná pro pájení a lepení.
Co snižuje bod tání hliníku?
Jedním z klíčových faktorů, které snižují teplotu tání hliníku, je přidání určitých prvků. Jak víte, hliník 7075 má nejnižší bod tání z celé rodiny. Pokud budete sledovat jeho chemickou strukturu, zjistíte, že obsahuje další prvky.
Jak ovlivňuje teplota hliník?
Teplota má na hliník významný vliv. Při vyšších teplotách je hliník měkčí. Měknutí má své výhody i omezení. Záleží především na konkrétních aplikacích.
Spojte se s námi!
If you have any questions, contact our customer support team. GC Mold is specializes in various aluminum cating parts and equipment. The company has the latest machinery for aluminum casting and extrusion. So, you are always welcome to our customer support for any aluminum service.
0 komentáøù